Avaliação da rugosidade superficial da zircônia (3Y-TZP) CAD/CAM após aplicação de três tipos de acabamento e polimento: estudo in vitro

Camila Ramos De Castro Gottardo
Doutora em Odontologia – Ulbra.
Orcid: https://orcid.org/0009-0004-6475-3471

Kalinka Crivellaro Crusius Schneider
Mestra em Cirurgia e Traumatologia Bucomaxilofacial – Ulbra.
Orcid: https://orcid.org/0000-0002-8283-6789

José Cícero Dinato
Doutor em Implantodontia – UFSC.
Orcid: https://orcid.org/0000-0002-8478-3879

Thiago Revillion Dinato
Doutor em Prótese Dentária – PUCRS.
Orcid: https://orcid.org/0000-0002-7663-0477

Luis Eduardo Schneider
Doutor em Odontologia e professor do curso de Odontologia – Ulbra.
Orcid: https://orcid.org/0000-0002-8428-2097

Ahmet Özkömür 
Doutor em Odontologia – PUCRS.
Orcid: https://orcid.org/0000-0003-4900-3731

Ricardo Smidt
Doutor em Odontologia – PUCRS.
Orcid: 0000-0002-0811-2774.

DOI: https://doi.org/10.71440/2675-5610.11.4.26.414-419.art

 

RESUMO

Objetivo: avaliar diferentes aspectos da rugosidade superficial da zircônia comparando três alternativas de acabamento e polimento. Material e métodos: 20 cilindros de zircônia foram divididos em quatro grupos: controle; azul (acabamento de borracha de granulação grossa); rosa (acabamento de borracha de granulação grossa e média); e cinza (acabamento com borracha de granulação grossa, média e fina). A área de superfície (Sa), a maior amplitude entre pico e vale (Rmax) e a rugosidade média (Ra) foram avaliadas através de microscopia de força atômica (MFA). Resultados: em Sa, todos os grupos apresentaram diferença estatisticamente significante entre si. Na análise de Rmax, os grupos controle e rosa diferiram de forma estatisticamente significante entre si e dos grupos azul e cinza. Já os grupos azul e cinza não diferiram de forma estatisticamente significante entre si. Na análise de Ra, os grupos controle e azul não diferiram de forma estatisticamente significante entre si, assim como o grupo rosa e cinza. Contudo, os grupos controle e azul diferiram dos grupos rosa e cinza de forma estatisticamente significante. Conclusão: os resultados apontam alterações na superfície da zircônia após o acabamento e polimento, reduzindo a rugosidade superficial da zircônia e gerando uma diferença estatisticamente significante sobre Sa. Em Rmax, houve uma diferença estatisticamente significante quando comparado o grupo-controle e os demais grupos. E Ra diferiu de forma estatisticamente significante do grupo-controle após a aplicação do acabamento e polimento nos grupos rosa e cinza. Estes resultados são fundamentais para a decisão de realizar o acabamento e polimento da zircônia.

Palavras-chave – Implantes dentários; Cerâmicas; Próteses dentais suportadas por implantes; Óxido de zircônia; Reabilitação bucal.

 

Evaluation of the surface roughness of CAD/CAM zirconia (3Y-TZP) after application of three types of finishing and polishing: in vitro study

Objective: evaluate different aspects of the surface roughness of zirconia by comparing three finishing and polishing alternatives. Material and methods: 20 zirconia cylinders were divided into four groups: control, blue (coarse-grit rubber finish), pink (coarse and medium grit rubber finish), and gray (coarse, medium, and fine-grit rubber finish). Surface area (Sa), maximum peak-to-valley amplitude (Rmax), and average roughness (Ra) were evaluated using atomic force microscopy (AFM). Results: in Sa, all groups show a statistically significant difference from each other. In the Rmax analysis, the control and pink groups differ statistically significantly from each other and from the blue and gray groups, while the blue and gray groups do not differ statistically significantly from each other. In the Ra analysis, the control and blue groups do not differ statistically significantly from each other, nor do the pink and gray groups. However, the control and blue groups differ statistically significantly from the pink and gray groups. Conclusion: the results indicate changes in the surface of the zirconia after finishing and polishing, reducing the surface roughness of the zirconia and showing a statistically significant difference in Sa. In Rmax, a statistically significant difference was observed when comparing the control group to the other groups. Ra differed significantly from the control group after the application of finishing and polishing in the pink and gray groups. These results are fundamental for the decision to perform finishing and polishing of zirconia.

Keywords – Dental implants; Ceramics; Implant supported; Zirconium oxide; Dental restorations.

 

Referências bibliográficas

  1. Bollen CM, Papaioanno W, Van Eldere J, Schepers E, Quirynen M, van Steenberghe D. The influence of abutment surface roughness on plaque accumulation and peri-implant mucositis. Clin Oral Implants Res 1996;7(3):201-11. https://doi.org/10.1034/j.1600-0501.1996.070302.x
  2. Rompen E, Domken O, Degidi M, Pontes AE, Piattelli A. The effect of material characteristics, of surface topography and of implant components and connections on soft tissue integration: a literature review. Clin Oral Implants Res 2006;17(suppl.2:55-67). https://doi.org/10.1111/j.1600-0501.2006.01367.x
  3. Rigolin MSM, de Avila ED, Basso FG, Hebling J, Costa CAS, Mollo Junior FA. Effect of different implant abutment surfaces on OBA-09 epithelial cell adhesion. Microsc Res Tech 2017;80(12):1304-9. https://doi.org/10.1002/jemt.22941
  4. Preis V, Behr M, Handel G, Schneider-Feyrer S, Hahnel S, Rosentritt M. Wear performance of dental ceramics after grinding and polishing treatments. J Mech Behav Biomed Mater 2012;10:13-22. https://doi.org/10.1016/j.jmbbm.2012.03.002
  5. Gautam C, Joyner J, Gautam A, Rao J, Vajtai R. Zirconia based dental ceramics: structure, mechanical properties, biocompatibility and applications. Dalton Trans 2016;45(48):19194-215. https://doi.org/10.1039/C6DT03484E
  6. Zucuni CP, Guilardi LF, Rippe MP, Pereira GKR, Valandro LF. Fatigue strength of yttria-stabilized zirconia polycrystals: effects of grinding, polishing, glazing, and heat treatment. J Mech Behav Biomed Mater 2017;75:512-20. https://doi.org/10.1016/j.jmbbm.2017.06.016
  7. Matzinger M, Hahnel S, Preis V, Rosentritt M. Polishing effects and wear performance of chairside CAD/CAM materials. Clin Oral Investig 2019;23(2):725-37. https://doi.org/10.1007/s00784-018-2473-3
  8. Petropoulos GP, Pandazaras CN, Davim JP. Surface texture characterization and evaluation related to machining. In: Surface integrity in machining. Springer; 2010. p. 37-56.
  9. Chi T et al. Surface texture analysis using stylus profilers. Veeco Instruments Inc.; 2004.
  10. Lin H, Yin C, Mo A. Zirconia based dental biomaterials: structure, mechanical properties, biocompatibility, surface modification, and applications as implant. Front Dent Med 2021;2:689198. https://doi.org/10.3389/fdmed.2021.689198
  11. Kaizer MR, Bano S, Borba M, Garg V, dos Santos MBF, Zhang Y. Wear behavior of graded glass/zirconia crowns and their antagonists. J Dent Res 2019;98(4):437-42. https://doi.org/10.1177/0022034518820918
  12. Riivari S, Shahramian K, Kangasniemi I, Willberg J, Närhi TO. TiO2-modified zirconia surface improves epithelial cell attachment. Int J Oral Maxillofac Implants 2019;34(2):313-9. https://doi.org/10.11607/jomi.6862
  13. Go H, Park H, Lee J, Seo H, Lee S. Effect of various polishing burs on surface roughness and bacterial adhesion in pediatric zirconia crowns. Dent Mater J 2019;38(2):311-6. https://doi.org/10.4012/dmj.2018-106
  14. Jungbauer R, Liebermann A, Hammer CM, Edelhoff D, Proff P, Stawarczyk B. Impact of polishing system on surface roughness of different ceramic surfaces after various pretreatments and bracket debonding. Clin Oral Investig 2023;27(8):4389-99. https://doi.org/10.1007/s00784-023-05058-3.
  15. Pfefferle R, Lümkemann N, Wiedenmann F, Stawarczyk B. Different polishing methods for zirconia: impact on surface, optical, and mechanical properties. Clin Oral Investig 2020;24(1):395-403. https://doi.org/10.1007/s00784-019-02953-6

 

 

Confira o artigo na íntegra: